Sunday, October 25, 2009

[MW:3541] Re: PT after root pass in SS welding

Hi,

There are PT pdts available for high temp...i GUESS at around 260 deg C

Best Regards

Vishal Mehta


Supertech Services Ltd.
Plot No A-253, Road No 30-B,
Wagle Indl Estate,
Thane 400 604.

Sent from my Nokia Wireless Device
-----Original Message-----
From: Mohamed Mubarak Syed
Sent: 25/10/2009 17:13:01
Subject: [MW:3539] PT after root pass in SS welding

Recently I faced the following issue and kindly clarify my doubt.
A qualified WPS for stainless steel (A312-TP304H) requires PT after root
pass.
After root pass, its not possible to perform PT immediately unless the
temperature reduces.
But, in normal practice,any weld is not to be stopped before completing hot
pass or 1/3rd of groove thickness.
I got difficulty in following both conditions on single weld joint.

Based on the above different opinions, kindly suggest me the right one with
details.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...