Monday, October 19, 2009

[MW:3520] Re: sour service

Dear

Nothing is absolute fact specially in metallurgy so i think that
your question is not a right question
in other words that Ni alloys are suitable for some appilcations and
not for other, and you have to search to find out your application
which alloy is suitable for it even it is not from Ni alloys

On Oct 18, 9:37 pm, "Owen Jenkins" <o...@osjl.co.uk> wrote:
> I think that is a misleading generalisation. There is a lot of excellent information available from the Nickel Institute free of charge, as downloads. All you have to do is search the site for what you want and register - it is entirely free. You can then download vast quantities of good and reliable information about nickel, its alloys, how to weld it, etc. I'd suggest you visitwww.nickelinstitute.org.
>
> Regards,
> Owen.
>
>
>
>   ----- Original Message -----
>   From: basem ali
>   To: materials-welding@googlegroups.com
>   Sent: Sunday, October 18, 2009 7:18 AM
>   Subject: [MW:3516] Re: sour service
>
>         Because Nickel is highly susceptible to stress corrosion cracking even with the presence of  a small amount of sulfide compound.
>
>         --- On Thu, 10/15/09, Ali Asghari <asghari...@rocketmail.com> wrote:
>
>           From: Ali Asghari <asghari...@rocketmail.com>
>           Subject: [MW:3506] sour service
>           To: materials-welding@googlegroups.com
>           Date: Thursday, October 15, 2009, 4:05 AM
>
>           hi all
>           why Ni is detrimental effect for corrosion property in sour service?
>           regards.- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...