Hello Gents

Can sombody help me with a answar regarding welding of Sa-335 to
SA-106.

I have a PQR covering material 335-P11 to 335-P11( P4)
Can I use it for welding of P-no 4 to P-no 1

Regard, jimmy

--~--~---------~--~----~------------~-------~--~----~