Hi,

 

Do you have sample of certificate type EN 10204 3.1 ?

 

Thanks

 

TRAN VAN VUONG

HP +84 912 262 085

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of K.M Hrishikesan
Sent: Monday, October 05, 2009 6:32 PM
To: materials-welding@googlegroups.com
Subject: [MW:3421] Re: Welding consumables certification

 

Hi,

 

Here's the difference

 

EN 10204 2.2 - Test report of Conformation of compliance with the order, with non specific test results and signed by manufacturer.

EN 10204 3.1 - Inspection certificate of Conformation of compliance with the order, with specific test results and signed by designated Quality personnel of the manufacturer independent of the production department.

Regards

Hrishi

On Mon, Oct 5, 2009 at 4:19 PM, ELAMARAN RAJAN <elams.rajan@gmail.com> wrote:

Dear Friends

 

As per our client specification for all welding consumables has to be minimum of EN10204 3.1 certification is required.

we are submitted EN10204 3.1 Chemical composition and for mechanical properties EN10204 2.2.

But Client not accepting that certificate due to mechanical properties has to be certified as per EN10204 3.1

 

let me know what is the difference between EN10204 3.1 and EN10204 2.2

regards
maran

 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...