[MW:3006] Re: Use of Butterfly valve in Natural gas storage plant ?

here are two comments from experts on the subject discussion, posted
elsewhere on the web,
____________________________________________________________________________________________
Hello Rahul,

I have used a lot of butterfly valves in gas processing application at
a reasonable high pressure level of approx. 30bar(g) and differntial
pressures of 20 until 25 bar.
The medium was hydrogen, syn gases, different feed gasses. These
butterfly's were used as block valves (manual and automatic) and in
high cycle service (cycling each 2 min).
The most important advantage is the smaller build-in dimensions and
the lower weight.
As you should select your ball valve, also for butterfly valves it is
extremly important to adapt the material characteristics to the
applicable operating parameters. But after more then 10 years of
experiences in use in this kind of applications, butterfly valves are
more and more used with very good results (also for leak tightness)

Regards,

Gino De Landtsheer
By Gino De Landtsheer Piping expert @ Borealis
posted 9 days ago | Delete
_______________________________________________________________________________________________
Rahul,
I have seen butterfly valves in use in the natural gas industry as
block valves on large distribution systems. When sizing control valves
with high efficiencies in design cv, noise and vibration need to be
considered.

Regards,
Brian Taylor
By Brian Taylor Mechanical or Industrial Engineering Professional
posted 2 days ago | Delete
______________________________________________________________________________________________
On Aug 14, 5:05 pm, nandakumar pandit <pandit...@gmail.com> wrote:
> request you to give pressure and temperature and expected no. of cycles. we
> have used butterfly valves at 60 degree C and 3.5 kg/cm2 pressure without
> adverse effect for on/off service.
> the valves were cycling every 15 min.
>
> nspandit
>
>
>
> On Thu, Aug 13, 2009 at 5:49 PM, <rahul.pi...@akersolutions.com> wrote:
> >  Hello all,
>
> > My question is not exactly related to material & welding , but it relates
> > to Valve application. I would very much appreciate your views.
>
> > I like to ask you all, does anyone has a experience of using Butterfly
> > valve, instead of Ball valve , in Gas processing / storage plant ?
>
> > I am studying possibility of using  Triple eccentric butterfly valve in
> > high pressure gas plant , instead of Ball valves.
>
> > Of course , there is no need of Pigging for these lines and    low Cv
> > values of butterfly valves are also in consideration.
>
> > Are there other design, operational,  process  parameters that limits the
> > use of butterfly valves for use in Natural Gas plants ?
>
> > Waiting for your guidance.
>
> > Kind regards
> > *Rahul Pisat*
>
> > This e-mail and any attachment are confidential and may be privileged or
> > otherwise protected from disclosure. It is solely intended for the person(s)
> > named above. If you are not the intended recipient, any reading, use,
> > disclosure, copying or distribution of all or parts of this e-mail or
> > associated attachments is strictly prohibited. If you are not an intended
> > recipient, please notify the sender immediately by replying to this message
> > or by telephone and delete this e-mail and any attachments permanently from
> > your system.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

The worth of butterfly valves as control valves has been escalating for the reason that the pressure loss is lesser than other kinds of valves and solidity is indeed very advantageous during installation. These qualities are advantageous for saving power and high effectiveness of devices.

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...