Dear viral,
Best suitable material for caustic service is Carbon steel with stress releived(PWHT)
all the weld joints to be stress releived even small bore piping, socket welding etc.
On 8/5/09, viral <viral.mech85@gmail.com> wrote:
Dear sir,
I want to know the most suitable material of piping or tank or etc. of
caustic service.
can u please advise me for above topic.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com