Monday, August 3, 2009

[MW:2867] RE: 2864] cladding

If the Clad is on CS/LAS To confirm complete removal of clad, apply Coper sulphate solution  on this area . Surface turns redish , It confirms that there is no contamination of clad is left over

 

Regards

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohammad Javeed
Sent: Monday, August 03, 2009 8:34 AM
To: materials-welding@googlegroups.com
Subject: [MW:2864] cladding

 

Dear all

I have one query about cladding. In our GTL project slug catcher is going on with construction code of B31.8. We have one pipe line of material 1SO 3183-3 L450 MCS with 3mm inconel cladding. As per our method statement we should require minimum 5mm de- cladding from the bevel edge before fit-up with machining or grinding.

So my question is, how we conform or ensure that cladding material is removed or not?

 

Regards

M JavedĂ‚ 



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...