You may find information about duplex and super duplex stainless
steels in the specifications EN10213 edition 2007. and SEW 410 edition
1998 (Stahl und Eissen Werkstoffblatt)
Regards,
Herman Pieper
On 30 apr, 15:58, daniel iordache <daniel.iorda...@gmail.com> wrote:
> Hello,
>
> Would you like to give me some details or mat. specification about 22%
> Cr duplex and 25 Cr Duplex ......
>