Monday, May 4, 2009

[MW:2098] RE: 2071] Duplex spec

Dear Daniel,

 

Refer the below link for Duplex & super duplex stainless steel applications & Mechanical & chemical properties.

 

 

http://www.pmfirst.com/duplex.php

 

Regards

 

Somesh Kumar Pandey

KBR Energy & Chemicals

79 Anson Road #20-01

Singapore 079906

Office: +65 6210 7459

Fax: +65 6210 7250

Email: Somesh.Kumar@kbr.com

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of daniel iordache
Sent: April 30, 2009 9:58 PM
To: materials-welding@googlegroups.com
Subject: [MW:2071] Duplex spec

 

 

Hello,

 

Would you like to give me some details or mat. specification about 22%

Cr duplex and 25 Cr Duplex ......

 

thanks

 

 


This e-mail, including any attached files, may contain confidential and privileged information for the sole use of the intended recipient.  Any review, use, distribution, or disclosure by others is strictly prohibited.  If you are not the intended recipient (or authorized to receive information for the intended recipient), please contact the sender by reply e-mail and delete all copies of this message.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...