Wednesday, March 4, 2009

[MW:1701] RE: 1697] RMD Process( Gas Combination)

Best combination is 75%Argon & 25%co2.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of gupta
Sent: Tuesday, March 03, 2009 5:14 PM
To: Materials & Welding
Subject: [MW:1697] RMD Process( Gas Combination)


Dear all
Can any body tell me that what is the best gas combination for
shielding with RMD process?

Thanks and B.regards
M.R.Gupta
AWS/CWI

-----------------------------------------
----------------------------------------------------------
This transmission is CONFIDENTIAL and the information is intended
only for the use of the individual or entity to whom it is
addressed. If you are not the intended recipient, or the employee
or agent responsible for delivering it to the intended recipient,
you are hereby notified that any use, dissemination, distribution
or copying of this communication is STRICTLY PROHIBITED. If you
have received the transmission in error, please immediately notify
us by email and/or telephone, and delete the transmission and any
attachments from your mailbox. Thank you.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...