Friday, October 24, 2008

[MW:1236] Hydro test-max holding period

As per B31.3 Hydro test is carried out at 1.5X Design Pressure.Holding
time for Piping spools is normally 30 minutes but at times 4-6 hours
for Gas applications.Can this be held for 24 hours?What is the
potential risk?It is normally indicated that after Hydro inspection
for 10-30 minutes at 1.5X Design Pressure,if you intend doing further
inspection then same can be done at a pressure not more than the
design pressure.Opinion of the group is being sought thro this mail
Regards
Aarpee

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...