Skip to main content

[MW:1242] RE: 1240] Which WPS can be used

it depends on after treatment of this weld, is this weld required or subjected to PWHT?
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of kataiah@bilfal.com
Sent: Sunday, October 26, 2008 9:38 AM
To: materials-welding@googlegroups.com
Subject: [MW:1240] Which WPS can be used


Dear Frinds ,

I have a requirement to weld  Stress relievedCS  plate # normal CS Plate.

Which WPS can is use to weld such combination ( i mean a WPS with PWHT or with out PWHT).

ASME is refering anywhere which type to be used?

What is the logic to use perticular type?.

Regards

P.K.
Bilfal Industries.

  --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...
CONFIDENTIALITY NOTICE
This e-mail and any attachments there to contain information, which is confidential, proprietary, privileged and/or protected from disclosure by intellectual property rights and are intended for the sole use of the recipient(s) named above. If you are not the intended recipient of this message you are hereby notified that any dissemination or copying of this message is strictly prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete it from any computer. Although this e-mail and any attachments thereto are believed to be free from any virus or other defects, which might affect any computer or IT system, it is the responsibility of the recipient to ensure that they are virus free. We are not liable for any loss or damage arising in any way from receipt or use there of. Thank you.