[MW:1235] Developing Welding procedures for sour service - Case history.

Controlling the hardness of the weld HAZ in sour service is essential to help prevent SSC. It is important to evaluate HAZ properties when developing welding procedures. The behavior of specific alloys during welding presents roadblocks to HAZ hardness control. The two cases referred in the attachment shows that weld thermal simulation is an efficient tool for developing welding procedures for sour service.

Source: MP October 2008.


<<Developing welding procedures for sour service.pdf>>

CONFIDENTIALITY NOTICE
This e-mail and any attachments there to contain information, which is confidential, proprietary, privileged and/or protected from disclosure by intellectual property rights and are intended for the sole use of the recipient(s) named above. If you are not the intended recipient of this message you are hereby notified that any dissemination or copying of this message is strictly prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete it from any computer. Although this e-mail and any attachments thereto are believed to be free from any virus or other defects, which might affect any computer or IT system, it is the responsibility of the recipient to ensure that they are virus free. We are not liable for any loss or damage arising in any way from receipt or use there of. Thank you.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...