Re: [MW:16499] Weld overlay/cladding WPS...

No --Disimilar metal butt Joint PQR can not qualify for Corrosion resistance Overlay
Regards
 
Hegde
From: Steven Teo <bvsteo@yahoo.com.sg>
To: materials-welding@googlegroups.com
Sent: Saturday, 12 January 2013 10:12 AM
Subject: [MW:16489] Weld overlay/cladding WPS...
Can WPS "V-groove weld details"of welding dis-similar material joints (eg..between CS and SS) also qualify for weld overlay or clad welding ?
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.  

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...