Hi,
means if welder is qualified in one of P1 to P11, P34, P41toP49 (homogen P number material) he's qualified to weld all homogen material Pnumber P1 to P11, P34, P41toP49. Just take care of others essential variables.
Regards
--
-- means if welder is qualified in one of P1 to P11, P34, P41toP49 (homogen P number material) he's qualified to weld all homogen material Pnumber P1 to P11, P34, P41toP49. Just take care of others essential variables.
Regards
2011/4/19 Srinivas Engr <srinivas.gmsrini@gmail.com>
Dear All,
as per ASME sec 9,
For welder qualification,
as per QW -350, P-Numbers are essential variable.
so change in p number needs to requalified.
& G-Number is not an essential variable. its no issues with G-Number.
1) My question is the above said are right or not..?
If any correction. pl let me know...
Q2) & is the welder qualified to weld P1 to P11, P34, P41 to 49.?
clear me on above issues..
Thanks & Regards
Srinivas
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments