Tuesday, April 5, 2011

Re: [MW:10600] UT OF PARTIAL PENETRATION JOINT OF STRUCTURAL WELD

Yes it is possible..
 
You can ensure the depth of fussion & root fussion(if required)
 
best regards,
 
msms
 


 
On Mon, Apr 4, 2011 at 10:55 PM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings....
 
Is it possible to perform UT of  Partial Penetration weld joint of beam with base plate.
 
construction code is AWS D1.1.
 
Thanks and Regards 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3