Re: [MW:10588] For 8mm/10 mm thick plate full penetration welding ,what will be the range qualified for pipe in fillet weld.
Please Refer
ASME Sec IX - QW-451 Procedure Qualification Thickness Limits and Test Specimens
On 25 March 2011 11:34, Venkateswaran <k.venkateswaran@ionexchange.co.in> wrote:
--If I conduct WPQ(SMAW or GMAW process,ASME SEC IX) for 8mm/10 mm thick plate full penetration welding ,what will be the range qualified for pipe in fillet weld.
Experts, can you Give reference clause form ASME SEC IX.
Thanks
kvr
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & Regards
Velan
Velan
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments