Google Groups
Subscribe to Materials & Welding
Email:
Visit this group

Monday, April 4, 2011

Re: [MW:10585] DPT for Structural welding

Hi
 
It has to specified by the contract spec.
 
Normally after root run not required incase of Structural welding by AWS D1.1, & 10% on final weld.
 
Thanks & Regards,
 
K. Babu
 

----- Original Message -----
Sent: Friday, April 01, 2011 7:35 PM
Subject: [MW:10573] DPT for Structural welding

Dear All
 
Can any body tell me if it is required to do DPT for root run & after final welding in structural steel. If yes how much percentage
 
CODE: AWS D1.1

--
Thanks & Regards
Feroz Mohammed
Deputy Manager-QA&I
LANCO Infratech Ltd.
È : +91 9650490097
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments: