[MW:10727] welding of super duplex stain less steel and critical pitting temp.

In our project during procedure qualification for super duplex stain
less steel we are not able to achieve the specified critical pitting
temperature.Welding conditions are

GTAW
ER2594
88%Argon+2%Nitrogen shielding gas
What we have to do to acieve the CPT

PLEASE REPLY

REGARDS

BIJU

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...