Skip to main content

Re: [MW:6527] RE: 6484] how can we differenciate between cs and kcs?

There are various method by which labs can check chemistry of the same, e.g. Optical Emission Spectroscopy (OES), ICP-OES and combustion analysis etc.
 
The laborartory is supposed to carry out this chemical analysis as a destructive test, so be clear on that before sending specimen to the lab.
 
Regards
Muhammad Bilal

On Mon, Aug 16, 2010 at 5:23 PM, John Henning <jhenning@deltak.com> wrote:
Typical x-ray fluorescence (XRF) instruments (Texas Nuclear, Niton etc.)
are not able to determine low atomic weight elements such as aluminum,
silicon, and carbon.  There are some field portable spark test
instruments (atomic emission spectroscopy - AES) that can.  Otherwise
you will have to send a test sample to have a laboratory analysis
performed - typically AES.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of aslam khan
Sent: Friday, August 13, 2010 11:45 AM
To: materials-welding@googlegroups.com
Subject: [MW:6484] how can we differenciate between cs and kcs?

dear friends ,
i want to ask a quaestion , how can we differenciate between cs and
kcs?if we do pmi ,then results are same ?is there any method by which
we can do differenciate between them?
thanks

regards
m.aslam khan
qa/qc engineer
descon engineering ltd.
engro site
cell#+923214217438

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Unknown said…
Actually, handheld XRF instruments (such as Thermo Scientific Niton Analyzers) do directly detect light elements down to Mg on the periodic table. You need an instrument with a silicon drift detector, or SDD. These analyzers can differentiate Al and Si killed steels from typical CS through direct detection of Al and Si. For example, a common use of Niton analyzers in petrochemical PMI is differentiation of A-106 (Si-killed) from A-53 based on Si content alone.

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...