Re: [MW:6478] GTAW for complete welding joint

I would add criticality of the weld


  From: Eng/ Mostafa Kamel Hussein [mkh_200@yahoo.com]
  Sent: 12/08/2010 00:36 MST
  To: materials-welding@googlegroups.com
  Subject: Re: [MW:6457] GTAW for complete welding joint


Full GTAW or any other welding process doesn't submit to any code, otherwise the client specification only can order you to do specified process so select the welding process depends on some factors as:
1- Type of material
2- Thickness of material and diameter ( Pipe Case)
3- Welding Position
4- Process Availability 
5- Process Cost
6- Production or site conditions

Regards,

SaSa 


From: Welder's Helper <vettaikkaran2011@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wed, August 11, 2010 12:29:06 PM
Subject: Re: [MW:6422] GTAW for complete welding joint

No code banned full GTAW operation on any metal and it is one of the best process in the world.We prefered SMAW due to economics.


--
Welder's Helper
 
Never bend my head infront of anyone other than GOD the almighty.

On Thu, Aug 5, 2010 at 7:14 PM, Mehmood Javed <mehmood.javed@fatima-group.com> wrote:
Dear All
Can we use GTAW only for complete welding joint in following  cases.
 
1- Pipe,  API 5L Gr B, 3" dia, Wall Thickness 10 mm
 
2- Pipe,  316-L (Urea Grade) , 3" dia, Wall Thickness 10 mm
 
 
Regards,
 
Asim
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...