[MW:6448] Re: Queries regarding the repair of castings

Dear Mr. Roy,

This depends fully on the base material specification. Most of the
material specifications prescribes repair procedures for minor and/or
major repairs or they refer to other specifications which are
applicable.
So you should first send some information about the material you want
to repair in order to send you a proper answer.

Best Regards

Herman Pieper

On 11 aug, 08:02, arijoy roy <bhai...@yahoo.com> wrote:
> Dear Sir
> I need the following informations
> 1) Which standards specifies the guidelines for repair welding of low alloy castings?
> 2) What is the depth, as a percentage of the total thickness, upto which repair welding is allowed?
> 3) What is the method of quality check of the repaired portion ?
> With Regards
> Arijoy Roy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...