Saturday, August 7, 2010

[MW:6353] Re: Hydrotesting of pipeline

Header material is API 5L grade X60

On Aug 7, 12:12 pm, sumit jaura <sumit.ja...@gmail.com> wrote:
> Dear all,
>
> Can anyone suggest that whether it is must to have radiography of all
> flanges and nipples on test header for hydrotesting?
>
> or we can only allow by ut or dpt only.
>
> Sumit ,
>
> P. engineer,
>
> Worleyparsons

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...