we are using a normal bend test method where we do the same on carbon steel.
the fracture is in the HAZ. so, even when you start bending it, it is broken straightway.
i would like to get more info about the changing of bend test methods.
best regards,
> Date: Tue, 2 Feb 2010 22:28:33 -0800
> From: wimvanhaver@yahoo.com
> Subject: Re: [MW:4193] Welding of Aluminum plate grade 6082 T
> To: materials-welding@googlegroups.com
>
> Dear Mr. Feyzullayev,
>
> Where does the fracture take place? In the weld metal or in the heat affected zone? Which kind of bend test are you using: three-point bend testing or wrap-around?
> If fracture takes place in the heat affected zone and you are using three-point bend testing: we have also had some experience with this in the past. Due to the severely softened zones in the HAZ, all deformation tends to take place in the HAZ. This produces a virtual former diameter which is significantly smaller than the actual former diameter. A solution to that might be to change your bend testing method (in agreement with your client, of course). Please let me know if you require more details about this.
>
> Kind regards,
>
> Wim Van Haver
> Belgian Welding Institute
>
> --- On Tue, 2/2/10, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:
>
> > From: Elshan Feyzullayev <elshan_f@hotmail.com>
> > Subject: [MW:4186] Welding of Aluminum plate grade 6082 T
> > To: materials-welding@googlegroups.com
> > Date: Tuesday, February 2, 2010, 3:55 AM
> >
> >
> >
> >
> >
> > Dear friends,
> >
> >
> >
> > I need to run the new WPSin Aluminium steel plate
> > using the attached grade of Aluminum plate.
> >
> >
> >
> > How many times I have tried but I can not get the
> > acceptable results from bend test.
> >
> >
> >
> > It is broken after slight bending.
> >
> >
> >
> > Can you help me please how to weld it to get the acceptable
> > results from bending?
> >
> >
> >
> > The wire I am using is ER5356 which is reccommended for
> > this type of AL.
> >
> >
> >
> > Best regards,
> >
> > Hotmail: Powerful Free email with
> > security by Microsoft. Get it
> > now.
> >
> >
> >
> >
> > --
> >
> > To post to this group, send email to
> > materials-welding@googlegroups.com
> >
> > To unsubscribe from this group, send email to
> > materials-welding-unsubscribe@googlegroups.com
> >
> > For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> >
> > The views expressed/exchnaged in this group are members
> > personel views and meant for educational purposes only,
> > Users must take their own decisions w.r.t. applicable
> > code/standard/contract documents.
> >
> >
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hotmail: Free, trusted and rich email service. Get it now.
the fracture is in the HAZ. so, even when you start bending it, it is broken straightway.
i would like to get more info about the changing of bend test methods.
best regards,
> Date: Tue, 2 Feb 2010 22:28:33 -0800
> From: wimvanhaver@yahoo.com
> Subject: Re: [MW:4193] Welding of Aluminum plate grade 6082 T
> To: materials-welding@googlegroups.com
>
> Dear Mr. Feyzullayev,
>
> Where does the fracture take place? In the weld metal or in the heat affected zone? Which kind of bend test are you using: three-point bend testing or wrap-around?
> If fracture takes place in the heat affected zone and you are using three-point bend testing: we have also had some experience with this in the past. Due to the severely softened zones in the HAZ, all deformation tends to take place in the HAZ. This produces a virtual former diameter which is significantly smaller than the actual former diameter. A solution to that might be to change your bend testing method (in agreement with your client, of course). Please let me know if you require more details about this.
>
> Kind regards,
>
> Wim Van Haver
> Belgian Welding Institute
>
> --- On Tue, 2/2/10, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:
>
> > From: Elshan Feyzullayev <elshan_f@hotmail.com>
> > Subject: [MW:4186] Welding of Aluminum plate grade 6082 T
> > To: materials-welding@googlegroups.com
> > Date: Tuesday, February 2, 2010, 3:55 AM
> >
> >
> >
> >
> >
> > Dear friends,
> >
> >
> >
> > I need to run the new WPSin Aluminium steel plate
> > using the attached grade of Aluminum plate.
> >
> >
> >
> > How many times I have tried but I can not get the
> > acceptable results from bend test.
> >
> >
> >
> > It is broken after slight bending.
> >
> >
> >
> > Can you help me please how to weld it to get the acceptable
> > results from bending?
> >
> >
> >
> > The wire I am using is ER5356 which is reccommended for
> > this type of AL.
> >
> >
> >
> > Best regards,
> >
> > Hotmail: Powerful Free email with
> > security by Microsoft. Get it
> > now.
> >
> >
> >
> >
> > --
> >
> > To post to this group, send email to
> > materials-welding@googlegroups.com
> >
> > To unsubscribe from this group, send email to
> > materials-welding-unsubscribe@googlegroups.com
> >
> > For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> >
> > The views expressed/exchnaged in this group are members
> > personel views and meant for educational purposes only,
> > Users must take their own decisions w.r.t. applicable
> > code/standard/contract documents.
> >
> >
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hotmail: Free, trusted and rich email service. Get it now.