Re: [MW:34203] Impact Testing requirements for PQR

Please provide below details

1. MDMT (minimum Design Metal Temperature)
2. Involved Material Grades like ASTM A105 / 106 Gr.B / 333 Gr.6  etc..
3. Applicable design code Like ASME B 31.3
4. Material thicknesses

Thanks & Regards

J.Gerald Jayakumar




On Monday, 8 May, 2023 at 06:49:53 pm IST, Jackson Raj <jacksonraj007@gmail.com> wrote:


Dear all

Is it mandatory to do Impact Testing in PQR our clients doesn't approaching to us to do Impact Testing they only required impact Testing in Forging Material Tee and flanges.

That's why we are doing Impact Testing in PQR.

Thanks & Regards
Jack

On Fri, May 5, 2023, 6:18 AM Srinivas Rao <srinivas.nitt11@gmail.com> wrote:

in addition to above one may consider PWHT requirements if anything applicable as per the design and client spec, if PWHT applicable one may consider additional PQR's or based on the construction code exemption recommendations PQR's Can be avoided by following pre-heat requirements of the construction code.

Regards, 
Srinivas Rao
On Thursday, May 4, 2023 at 3:22:12 PM UTC+4 james gerald wrote:
Appreciate efforts and initiative from ENG.Ahmed.

Just to share. 2 PQR's 6mm & 23mm is sufficient.

There is an ASME Interpretation stating PQR qualified on 6mm and higher thickness qualifies in the range from 16mm.  Someone please share the Interpretation.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 4 May, 2023 at 03:45:32 pm IST, 'Ahmed Osman' via Materials & Welding <material...@googlegroups.com> wrote:


3 PQR's may be sufficient , 6mm (3-12) 10mm (10-20) 23mm (16-46) 

Best Regards ,
ENG. Ahmed Osman



On Wednesday, May 3, 2023 at 08:44:46 a.m. GMT+3, Jackson Raj <jackso...@gmail.com> wrote:


Dear all,

In Our project has 3 inch to 24 inch and it's thickness 5.49mm to 45.24mm and Impact Testing required for above thickness.
Please clarify how many PQR are required for this job 
Please consider the Impact Testing also mentioned each PQR thickness qualify 

Regards
JJ

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaXAKmJFBKLz39ZoUn%3Dnwi4Er11Qts17%2BbWyQkBOYML4Eg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95dfb447-8b39-4c0b-a898-6f5683be32ecn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaV79Dt0jr5nNzR1f75utkFDJ6U2mh7rSjS52R9o_ko_Cw%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...