Re: [MW:34249] Chinese Steel to ASME BPVC Compliance

Dear Fernando

QW 422 ASME SEC IX 
This table enlists  P no Gr for specified materials .
For ASME SEC IX PQR  ,only LISTED materials are permitted to take range of qualification.
Unlisted materials ( Not listed  in QW 422 Table)need separate qualification.

For WPQ  , the Welder qualification can be done on other NON ASME materials with matching chemistry , Strength with ASME Listed materials Pl speak to AI for WPQs for unlisted material for WPQ.Any Client permission  . You may have to take or keep apprised about the same .

Thanks 

Vishwas IWE


Sent from my iPhone

On 31-May-2023, at 8:37 AM, Fernando L Neto <fernando.lescovar@gmail.com> wrote:


Hello, dear friends. I hope this email finds all of you well. 

Considering that there is a list of steels (and other metals) that are listed by the ASME BPVC Code, and also considering that there is a large list of steels produced that are not included in this official list, what are the steps to be taken to establish an equivalence and reclassify a steel such as Q235B (Chinese) to SA36 (I don't think it's only due to chemical composition and mechanical properties)

Any help will be very much appreciated. 





Não contém vírus.www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANv%2BETbuUKV2mzD657vAfH751isA%3Dhr%2Bz2g%2BfZe6aTsNW0Q-Zw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...