Skip to main content

Re: [MW:34239] ER80S-G/ER80S-Ni1

What is the composition of 
ER80S-G
ER80S-Ni1

Send   MTCs  of both  the consumables

On Tue, May 23, 2023 at 1:20 PM Baqer Shabbeer <engbaqer@gmail.com> wrote:

Dear experts,

I would appreciate your valuable response regarding the following inquiry.

The filler wire mentioned below is approved for our normal Gas Metal Arc Welding (GMAW) Welding Procedure Specification (WPS):

·        AWS Classification: ER80S-G

·        SFA Specification: 5.28

·        API 1104 Group: 5

·        Trade Name: PIPELINER 80Ni1

·        Base metal API 5L Gr. X65

However, for repair welding joints, our approved WPS (GMAW Welding) specifies the use of the following filler wire:

·        AWS Classification: ER80S-Ni1

·        SFA Specification: 5.28

·        API 1104 Group: 5

·        Trade Name: PIPELINER 80Ni1

·        Base metal API 5L Gr. X65

Unfortunately, my team used AWS Classification ER80S-G for the repair welding using Repair WPS.

I would like to know if this deviation is acceptable or if any corrective actions are necessary.

Thank you for your expertise and guidance.


Regards,

Baqer


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/30a48598-af6d-4f67-9b81-dcd6e1d9f3a1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OFzmNAi8btPaUzrmXcLhRrjmaT_v5%2BzFLTnv6wCeaRZA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .