Skip to main content

[MW:34252] RE: 34251] Re: PQR WITH TWO WELDING PROCESS TO SEPERATE IT

Yes its possible, You can go for only SMAW considering all other essential variable

 

QW-200.2(f) One WPS. Several WPSs may be prepared from the data on a single PQR (e.g., a 1G plate PQR may support WPSs for the F, V, H, and O positions on plate or pipe within all other essential variables). A single WPS may cover several sets of essential variable ranges as long as a supporting PQR exists for each essential and, when required, supplementary essential variable [e.g., a single WPS may cover a thickness range from 1/16 in. (1.5 mm) through 11/4 in. (32 mm) if PQRs exist for both the 1/16 in. (1.5 mm) through 3/16 in. (5 mm) and 3/16 in. (5 mm) through 11/4 in. (32 mm) thickness ranges].

 

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of biennd
Sent: Wednesday, May 31, 2023 12:15 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:34251] Re: PQR WITH TWO WELDING PROCESS TO SEPERATE IT

 

Hi there,

 

May you check in which standard refers to.

I understood, ASME IX allowed for thickness of test coupon more than 13 mm.

 

Thanks

Bien ND

 

On Tuesday, May 30, 2023 at 6:28:48 PM UTC+7 QA/QC wrote:

Dear master 

 

please can you advise me i have some doubt 

in our project i have a PQR qualify with gtaw + smaw butt weld 

Detail :

 

7.14 to 20 (CS & LTCS)
GTAW  5 mm +SMAW 9
ER70S-6 + E7018-1 

 

and i want to qualify to only SMAW PROCESS is it possible or no 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8e67b12e-4012-4530-91ce-7940fb52f5d6n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .