Dear Ilkin,

 

The alloy 625 (Ni-Cr-Mo-Nb) for high temperature service 0-800 C and highly corrosive environment, rarely requires impact testing. ASTM B564 (UNS NO6625) does not state it as proof of its mechanical properties. If this is your case, at what temperature would you perform the Charpy test?

Better: in what temperature range is the service of this alloy located, in your case?

 

Regards,

Ramon Briceno.

 

 

 

Sent from Mail for Windows 10

 

From: Ilkin Hasanov
Sent: Wednesday, March 31, 2021 6:25 AM
To: materials-welding@googlegroups.com
Subject: [MW:32130] Charpy Test of Inconnel (ASME B 31.3)

 

Hi All,

Could you please advise, when does ASME B31.3 require to perform Charpy Test for Inconel Material (UNS 06625)? 

 

After which MDT it is mandatory to perform it? 

 

 

Regard, 

Ilkin HASANOV.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYXdxMbYXHYBV%2BRaKidjv7B%2BB_x7%3Dw8Mz5h1k-Nm%2BfiQg%40mail.gmail.com.

 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...