Thursday, April 1, 2021

[MW:32137] A335/SA335 - P 9 MATERIAL PQR AND WPS

Dear experts
One of my friend asked me a copy of PQR and WPS of A335/SA335 P 9 material.
If anyone is having,please share the same.
Thanks and regards
Sampath

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFvB4b6%2BKPQ--uw-4ME_YEdxewQ%2BF7qehSu76b9R8%3DcZm5OJ_Q%40mail.gmail.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...