Dear Mr. Selvin,

Enclosing  two articles towards,
1. Preheating LAS and 
2. Relation between preheat & micro structure recently up loaded for your study.

The second article was published in the year 2019 in Springer Nature Journal and 
will give you an idea towards preheat and micro-structure relation.

Trust it will help you.

regds,
C Sridhar.
-------------------------------------------------------------------------------------------------

On Friday, 28 February, 2020, 04:36:31 pm IST, selwin jebadas <selwinjebadass@gmail.com> wrote:


Experts,

I need some basic understanding from LAS welding.

1)Need for preheat in LAS?
2)Preheat & microstructure relation?

Many thanks,
Selwin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJe433Md_wcr2%2BpdqyRJC94iULZomWNUZAzGHVby4HvWD_P2Dg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...