Thursday, February 27, 2020

Re: [MW:30553] PWHT

Material of construction may be ASS??

On Wed, 26 Feb 2020 8:28 pm prateik tolani, <tolaniprateik@gmail.com> wrote:
Dear Experts,

one of our client is asking for Solution annealing for complete vessel
vessel size - 1300 ID x 6500 mm long, thickness 8 mm with lots of nozzles.
whether it is possible.
at higher temperature of 1100 Deg C and rapid cooling in water, vessel will distort completely.


Tolani 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_B7ijqhsdu07O8_05RXO4bHD8%3D%2BGpUx9W68j--H_ZMXQQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNcpCcbL0ANDN4LjbtwcFvfF_dWfaQ6vV7feVpi_KBpWQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...