U have to do like sprinkle type flow on the vessel. Do not immerse or forced water flow on the because it will get collapsed. Be cautious in designing your type of water flow. It is very important. 

On Thu, 27 Feb 2020 8:54 am harenath jha, <harenathjha@gmail.com> wrote:
Material of construction please

On Wed, Feb 26, 2020, 20:28 prateik tolani <tolaniprateik@gmail.com> wrote:
Dear Experts,

one of our client is asking for Solution annealing for complete vessel
vessel size - 1300 ID x 6500 mm long, thickness 8 mm with lots of nozzles.
whether it is possible.
at higher temperature of 1100 Deg C and rapid cooling in water, vessel will distort completely.


Tolani 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_B7ijqhsdu07O8_05RXO4bHD8%3D%2BGpUx9W68j--H_ZMXQQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UPY0TME2yjh2Dxz1o5mP_jBS1DD4%2Bimotd3rBsmy_HGUQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNZczkcfxTYWjdBQD_KTCnxpZ9-nM6iOjegUgXb%3D5o7%2BA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...