Re: [MW:30533] HIC Resistant Material - EIL Specification

Hi,

I am not sure about EIL requirements.

Normally Forgings and Seamless pipes do not require HIC testing requirement as the these production methods eliminate many discontinuities(impurities) which cause HIC.

Only plates are to be tested for HIC testing to Client Specifications or to ISO TM0284. Pipes rolled from plates also require this testing.

Regards,
Albert R


Sent from Yahoo Mail for iPhone

On Friday, February 21, 2020, 2:20 PM, sagar bogwad <sagarbogwad@gmail.com> wrote:

Dear Experts,

Need your expert advise on below :

Background :
Equipment data sheet specifies HIC resistant material to be used.
And applicable EIL specification 6-79-0013 R1 (Material requirements for Carbon steel components used in Sour service for petroleum refinery environment)
I understand these specification calls for HIC testing of Plates & Rolled products(pipes fittings made from plates) only.

Question :
Does EIL Specification 6-79-0013 R1 calls for HIC testing of components other than plates & rolled products such as Forgings, pipes, fittings, fasteners as well?

Kindly confirm with clarifications for better understanding.


Best Regards, 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiDOxk%3DNOyKmTeY%3DdPa1WTvc%2Bw51q0M1AbsANrqFL5fXwzPhg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...