Re: [MW:30498] Re: Welder Qualification in 3G position by 1G PQR

Ref please

On Tue, 18 Feb 2020 6:03 am NARK, <nidhin595@gmail.com> wrote:
As per the ASME SECTION IX-ED-2019,the position is not a essential variable but AWS D1.1 limits position,it depends up on the applicability.


Regards

Nidhin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38a6950d-8f08-4d14-892c-f8a6587d626e%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM%3DM8bJTcD27bd83Xfu6T-EiZMqi%3DskdkYSSzVBMx0oHA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...