Wednesday, February 12, 2020

Re: [MW:30480] FCAW process for U stamp vessel

It'scorrect I have experienced Root LOF found all the way. Bcoz of high weld metal deposition rate Double V ideal case or Back gouging is required. 
Regards, 
S.SENTHILKUMAR 


On Wed, 12 Feb 2020 at 7:00, Ramesh
<rameshkannandevaraj@gmail.com> wrote:
The FCAW restrictions  as below 


 

The FCAW Gas Shielded process shall not be used for the root pass on full penetration, groove joints that are welded from one side only without backing

 

The FCAW   self-shielded shall only be permitted prior approval through pWPS with full matrix of proposed testing



Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Feb 12, 2020 at 9:23 AM Chintan <chintan51@gmail.com> wrote:
Kindly advice

in general major clients write in thier specs FCAW process not allowed in presure vessel & pressure pining joints

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/926b0970-558d-47f7-8c53-3de21d008787%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcGnn%3DKfEiXm_vD6wnuP-czLfiYKPwhbPr8k3b9sPPfO1Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/602681480.1490624.1581487711760%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...