Thanks for info
Sharing result of my PQR
I run PQR with EH12k & neutral flux & got F8A3 mechanical property
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/097e29cd-f8b8-49c4-8733-acb549a89cec%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon
Hi As its %elongation is very low Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-