[MW:30541] Welding of Cladded plate of SA36+Alloy C276 with SA36+Alloy C276

Please help for developing welding procedure for below details:-
Absorber Tank Plate material - Cladded plate (SA36+Alloy C276) with (SA36+Alloy C276)
Thicknesses - 10mm(8mm-SA36 & 2mm-C276)
                        14mm(12mm-SA36 & 2mm-C276)
                        22mm(20mm-SA36 & 2mm-C276)
                        27mm(25mm-SA36 & 2mm-C276)
Kindly suggest weld joint design, Welding Process, Filler wire specifications, Type of test required for procedure development.

Kindly help in this regard as I'll be highly obliged

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/32419eda-0c04-4462-8663-3d58d846def2%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...