Dear Experts,
For SA 182 F11 and SA 182 F22 materials after welding and PWHT hardness of Base Metal is reduced to 120 HB, is it acceptable or not ?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/abc35094-fc8b-4ed9-93a7-69bcac2d1b1c%40googlegroups.com.
For SA 182 F11 and SA 182 F22 materials after welding and PWHT hardness of Base Metal is reduced to 120 HB, is it acceptable or not ?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/abc35094-fc8b-4ed9-93a7-69bcac2d1b1c%40googlegroups.com.
Comments