Tuesday, September 24, 2019

Re: [MW:30090] Re: PQR for PTAW Process by ASME Sec IX

It is important that you mention what the Construction Code is

El mar., 24 sept. 2019 a las 4:48, Bien_ND / weldinginspections.net (<bck055@gmail.com>) escribió:
please run follow machine manual and consumable manual.
I did a procedure PTA with Dura-Metal as them instruction.


On Monday, September 23, 2019 at 10:24:23 AM UTC+7, sathis...@gmail.com wrote:
> Dear Experts
>
> I would like to know below query on preparation of PQR as per ASME Sec IX, Process: PTAW by hardfacing overlay by Stellite 6 Powder
>
>
>
> 1. What is the current, voltage, Gas flow and Powder feed rate need to be maintained for 10mm and 25mm thickness plate. To which standard and reference i need to refer.
>
>
>
> 2. What is the pre heating and interpass temperature need to be maintained for P.No: 1,8,4,5A, 15E and to which standard need to refer
>
>
>
> 3. What is the hardness requirement for P.No: 1,8,4,5A, 15E during testing PQR? Which standard is mentioned this requirement?
>
>
>
> 4. Chemical analysis is mandatory for Co base as per ASME Sec IX , Table QW: 453
>
>
>
> Kindly give your suggestion and feedback for the above doubts
>
>
>
> Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26d6e35c-4e74-4687-a9b1-425343919b7e%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLugykWuW1QJrM2_-8eG0pJUu6jEr0XymRiR4N6SBXkEQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...