Thursday, September 19, 2019

[MW:30078] APPENDIX R OF ASME B31

Dear All.

in Appendix R of B 31.3 said that mentioned criteria is based on fracture mechanic without doing CTOD or considering of fracture property of material.how is it possible?because in similar standards that want to establish a acceptance criteria against workmanship need to be known this properties for each material.

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7c3a2438-1166-451b-b02d-6601ab4c63ee%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...