Re: [MW:30015] SAW Hardfacing maximum thickness

Generally its coming 3-4 mm.

On Sep 1, 2019 10:14 AM, "Weldbro" <itsashishwalia@gmail.com> wrote:
Can anyone suggest what is the maximum single layer thickness that can be achieved in SAW hardfacing. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39f9b768-7fa6-47d9-a09c-4aaf59a22e19%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrVsVVeqsEnpyu9bRz-S4-%3DLsTjPKqJJ%2BpPQ6FrYsvZd-w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...