Re: [MW:30066] Diameter qualified for set in nozzle

refer IX-80-67

On Mon, 16 Sep 2019 at 12:56, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gents, 

Is there any interpretation available for set in type nozzle welding diameter not essential variable for welder qualification?.

Reg

-- 

--