Re: [MW:30039] Welding of Alu With SS

No

On Mon, 9 Sep 2019, 9:03 am Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Is it possible in fusion welding???

On Mon, 9 Sep 2019 9:24 am Hani Al Masry, <hanyonalfy@gmail.com> wrote:
What is the electrode and MIG wire for welding SS pad eyes 316L with Aluminium pipe 6063

Regards 
HA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzd-9_7A%3DnSc19nLCLWt7SgVzLV68SOgqOMr7hRkqRgxEA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMi_NwYi9R4o8fAKKrQnP9C8xZTDrhD011N%2B2DhPchJpw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzcSRNKrvjubT9qM0qNp5UpNWzeE2OnnA6S%2Be6T3tiM35Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...