Dear experts,
EN AW 5754 H22 welded with ER5356, RT clear but gets failed in tensile.
What can be the reason please guide..
The artilce wleded is a 3 mm thick plate to plate butt joint.
Required YS 0.2 - 130 MPa
I am getting only 103 and 99 MPa.
Required UTS - 220-270 MPa
I am getting - 213 & 205 Mpa
Regards
Kadir godil
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/095b8b80-596a-4a0c-9cce-f2da1cbb7972%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment