make single pqr with 2normalizing + pwht

On Monday, 12 August 2019 15:44:19 UTC+5:30, chiluka venkatramulu wrote:
Dear All,
Pl clarify the below.
One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
  • Dishends Normalising-2 cycle.
  • PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?
OR
Only two normalising cycles are enough?

Regards,
Venkatramulu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dbd87a00-dfc9-4a38-984b-64476f767664%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...