Re: [MW:30025] Change groove type in D1.1

Yes,  you can change as joint design is non essential variable. 

Regards, 
Chandan Sharma 

On Thu 5 Sep, 2019, 8:45 AM hoàng nguyễn, <nhathoangbk286@gmail.com> wrote:
Dear Experts,

Could you please advise me for a question:
I have a PQR qualifies single V, can I write WPS for single V, doubleV, single Bevel, double Bevel.

Thank Experts

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM8%3DVVG6wmP0-XVh9jNLDqre4vs_wjZK-NNSYUmKwRjNyfsx5w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTWUJK5qacoYpWzm78L5eT6QWdLuVrieVy7TWJvrCEKwhgahQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...