Re: [MW:30040] Annular plate

Dear, sangram

What the meaning of radial joint ?

Thanks for your cooperation 

On Mon, Sep 9, 2019, 07:53 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Basem
Yes as per API-650 you need to be radiograph at least one spot on 50% of total joints.

Regards 
Sangramkeshari Routray 
Welding inspector 

Sent from my iPhone

On 07-Sep-2019, at 12:08 AM, basem elabd <eng.basem.elabd@gmail.com> wrote:

Dear all

Are the but welding joint in annular plate of tank must be RT or not as per API 650?

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACct1WHdS23%2BJ-gP9DybDPqfOqqUKDssOugYqYAjrY%2B8zYrEgg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/890DE5AF-2731-4DD0-888E-3D0625358EFC%40yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACct1WF4-%2BVWE5By%2BpJGrdeT%3DL_GPqWZxEj1wPWQPV-ozFjdaQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...