Re: [MW:30048] Weep hole

The trapped burnt gases may be corrosive and corrode the weld joint and dummy pipe in due course.

On Tue, Sep 10, 2019 at 10:01 AM Raghul <raghul351991@gmail.com> wrote:
I know the purpose of weep hole

But what I am asking is,If weep hole not provided
What is the problem will come ??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/15875721-1a62-4559-a016-42b466fee392%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeBZdrTn08ED1x_rOtbUi6TVkmHMcLq69TA%2BPdUfmJ5e7Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...