API 5LD is not very clear on this, std needs a revision to address this along with other issues (there are many problems with this std). However, I would recommend you to perform UT for disbondment inspection as per the criteria laid in Clause 11.1 of API 5LD
On Thursday, August 15, 2019 at 10:13:56 PM UTC+5:30, neilash kumar wrote:
-- On Thursday, August 15, 2019 at 10:13:56 PM UTC+5:30, neilash kumar wrote:
GentsIs there UT mandatory as per API5LD? For claded product . Weld overlay on pipes.RegardsNeilashkumar